GCS Sludge
GCS Sludge

The principal function of ferroalloy addition is that it increases the resistance of steel to corrosion and oxidation, improves its hardenability, tensile strength at high temperatures, wear and abrasion resistance and increases its other properties like creep strength etc2.
Grade | Carbon | Silicon | Manganese | Sulphur |
---|---|---|---|---|
Basic Grade | 4.6 | 0.08 max | 1.00 max | 1.20 |
Basic Grade | 4.6 | 0.05 max | 1.25 max | 1.20 |
Basic Grade | 4.6 | 0.08 max | 1.25 | 1.20 |
Basic Grade | 4.6 | 0.07 max | 1.50 | 1.20 |
Basic Grade | 4.6 | 0.07 max | 1.50 | 1.05 |
Basic Grade | 4.6 | 0.07 max | 1.75 | 0.90 max |
Basic Grade | 4.6 | 0.07 max | 2.00 | 1.05 max |
We have launched Ferrosilicon (FeSi) in the market with Internationally accepted Grade (70% Si) with the production of lower grades as well.